Glass fiber grid cloth paste method is introduced


 Glass fiber grid cloth is based on the material of glass fiber woven, soaking by high child resistant emulsion coating.Which has a good alkali resistance, flexibility Latitude and longitude, and to the high tensile resistance, can be widely used in building internal and external wall thermal insulation, waterproof, crack resistance, etc.With alkali glass fiber grid clothGlass fiberNon-alkali net cloth is given priority to, it USESGlass fiberYarn (ingredient is silicate, chemical stability is good) by the special organization structure, leno weave organization, after alkali resistance, strengthening agent high temperature to finalize the design process.
Main USES glass fiber grid cloth is widely used in wall enhanced material (such asGlass fiberWall mesh cloth, GRC wall panels, EPS external insulation board, gypsum board, waterproof coiled material cloth, asphalt roofing waterproof, fire prevention board, building sealing belt and so on.
Glass fiber grid cloth paste method:
1, the preparation of polymer mortar must be someone who's in charge, to ensure that the mixing quality.
2, open the lid counter-clockwise, use the blender or other tool will binder to stir, avoid the separation phenomenon in a binder, mixing moderate, lest appear quality problem.
3, polymer mortar mix proportion is: the KL binder: 425 # : sulphur aluminate cement sand (18 mesh bottom) : = 1:1. 88:3.25 (weight ratio).
4, the dosage of cement, sand barrels according to pour into a groove in the iron ash mixed, mix according to the mixture ratio after adding binder, stir, stir must be uniform and avoid segregation, gruel.According to the workability can be appropriately adding water.
Five water, water for concrete.
Six, polymer mortar should be along with it, with good polymer mortar is best used within 1 hour.Polymer mortar should be in a cool place, avoid sunlight exposure.
7, according to the need to length, width, from the whole volume in advanceGlass fiberCutting a net net cloth, set aside the necessary lap length or the length of the overlap.
8, the place in a clean flat cut, the material must be accurate, cut good net cloth must be rolled up, are not allowed to fold, not allowed to trample.
9, Yang Angle place for strengthening layer from building to building, strengthening layer should be posted on the inside, 150 mm per side.
10, daub is the first time the polymer mortar, should maintain EPS board face dry, remove the plate cotton harmful substances or impurities.
11, on polystyrene surface a layer of polymer mortar, scraping the area should be slightly greater than net cloth by the length or width, about 2 mm thickness should be consistent, besides you have serging requirement, polymer mortar are not allowed to apply in polystyrene board side.
After 12, scraping the polymer mortar, network layout should be on it, the curved edge of the fabric is toward the wall, from central to wipe TuPing, embedded in the polymer mortar, so that the net cloth fabric should not buckling, treated surface, after dry again on it with a layer of polymer mortar, the thickness of 1.0 mm, net cloth should not be exposed.
13, mesh cloth around the lap length should not be less than 70 mm, at the site of the cut, mending their nets should be adopted for the lap, lap length shall not be less than 70 mm.
14, door to flirt around should be strengthening layer, strengthen layer grid it on the inside. If the door window frame from skin and wall surface at the grass-roots level greater than 50 mm, the grid cloth with wall paste at the grass-roots level.If less than 50 mm to do turn packet processing.Great Wall laid grid cloth should be embedded in the door window frame lateral glued down.
15, door window corners, in the standard net after the wipe out of the corners of the door window again with a 200 mm x 300 mm standard network, with a 90 degree Angle bisector window placement, posted on the outside piece, to strengthen;The shade in place with a 200 mm long and width of the optimal window bang width standard mesh, stick on the outside.
16, a layer under the window, in order to prevent the damage from the impact, should be reinforced net cloth, relocation standard mesh cloth.Should strengthen the grid cloth docking.
17, the resettlement of strengthened layer construction method is the same as the standard of screen.
18, metope stickup grid cloth should be covered in the package grid cloth.
19 from top to bottom, mesh cloth wipe, synchronous construction first wipe reinforced net cloth, do standard mesh cloth
After 20, mesh cloth glued should prevent the rains washed out or impact, easy to collision, the Angle of the doors and Windows protection measures should be taken, feeding mouth parts take pollution prevention measures, surface damage or contamination should be dealt with immediately.
Layer 4 hours after 21, construction can't be the rain.