Fiberglass mesh
Product Name:
Fiberglass mesh
:
:
:

Product Description:
 Glass fiber grid cloth is based on the material of glass fiber woven, soaking by high child resistant emulsion coating. Which has a good alkali resistance, flexibility Latitude and longitude, and to the high tensile resistance, can be widely used in building internal and external wall thermal insulation, waterproof, crack resistance, etc. Glass fiber grid cloth is given priority to with alkali resistant glass fiber mesh cloth, it USES the alkali-free glass fiber yarn (ingredient is silicate, chemical stability is good) by the special organization structure - leno weave, after alkali resistance, strengthening agent high temperature to finalize the design process.

Introduction to the:
 
On the alkali or alkali free glass fiber grid cloth weaving yarn, the alkali resistant polymer emulsion coating glass fiber grid cloth series products: alkali GRC fiberglass mesh cloth, alkali resistance wall enhancement, and stone Mosaic private networks, marble back grid cloth
 
Main use is widely used in:
 
(1) wall enhanced material such as glass fiber wall mesh cloth, GRC wall panels, EPS exterior insulation board, gypsum board, etc.
 
2) reinforced cement products (such as the Roman column, the flue, etc.)
 
3) private networks (VPNS), granite, Mosaic marble back stick network.
Glass fiber grid cloth
 
4) waterproofing materials, asphalt roofing waterproof.
 
5) reinforced plastic, rubber skeleton material.
 
6) fire prevention board.
 
7) grinding wheel base fabric.
 
8) road surface with geogrid.
 
9) used in sealing belt and so on.

The characteristics of:
1, the chemistry stability is good. Alkali resistance, acid resistance, water resistance, erosion resistance of cement, and other chemical corrosion resistance; Strong bonding, and resin soluble in styrene, etc.
 
2, high strength, high modulus, light weight.
 
3, good dimensional stability, stiff, smooth, not easy contraction deformation, positioning is good.
 
4, good toughness. Good impact resistance.
 
5, prevent mildew, insect-resistant.
 
6, fire prevention, heat preservation, sound insulation, insulation.
 
Used to introduce:
1, the preparation of polymer mortar must be someone who's in charge, to ensure that the mixing quality.
 
2, open the lid counter-clockwise, use the blender or other tool will binder to stir, avoid the separation phenomenon in a binder, mixing moderate, lest appear quality problem.
 
3, polymer mortar mix proportion is: the KL binder: 425 # : sulphur aluminate cement sand (18 mesh bottom) : = 1:1. 88:3.25 (weight ratio).
 
4, the dosage of cement, sand barrels according to pour into a groove in the iron ash mixed, mix according to the mixture ratio after adding binder, stir, stir must be uniform and avoid segregation, gruel. According to the workability can be appropriately adding water.
 
Five water, water for concrete.
 
Six, polymer mortar should be along with it, with good polymer mortar is best used within 1 hour. Polymer mortar should be in a cool place, avoid sunlight exposure.
 
7, according to the need to advance the length and width of fiberglass mesh cloth from the roll cutting a let down the nets, set aside the necessary lap length or the length of the overlap.
 
8, the place in a clean flat cut, the material must be accurate, cut good net cloth must be rolled up, are not allowed to fold, not allowed to trample.
 
9, Yang Angle place for strengthening layer from building to building, strengthening layer should be posted on the inside, 150 mm per side.
 
10, daub is the first time the polymer mortar, should maintain EPS board face dry, remove the plate cotton harmful substances or impurities.
 
11, on polystyrene surface a layer of polymer mortar, scraping the area should be slightly greater than net cloth by the length or width, about 2 mm thickness should be consistent, besides you have serging requirement, polymer mortar are not allowed to apply in polystyrene board side.

12, scraping the polymer mortar, network layout should be on it, the curved edge of the fabric is toward the wall, from central to wipe TuPing, embedded in the polymer mortar, so that the net cloth fabric should not buckling, treated surface, after dry again on it with a layer of polymer mortar, the thickness of 1.0 mm, net cloth should not be exposed.
 
13, mesh cloth around the lap length should not be less than 70 mm, at the site of the cut, mending their nets should be adopted for the lap, lap length shall not be less than 70 mm.
 
14, door to flirt around should be strengthening layer, strengthen layer grid it on the inside. If the door window frame from skin and wall surface at the grass-roots level greater than 50 mm, the grid cloth with wall paste at the grass-roots level. If less than 50 mm to do turn packet processing. Great Wall laid grid cloth should be embedded in the door window frame lateral glued down.
 
15, door window corners, in the standard net after the wipe out of the corners of the door window again with a 200 mm x 300 mm standard network, with a 90 degree Angle bisector window placement, posted on the outside piece, to strengthen; The shade in place with a 200 mm long and width of the optimal window bang width standard mesh, stick on the outside.
 
16, a layer under the window, in order to prevent the damage from the impact, should be reinforced net cloth, relocation standard mesh cloth. Should strengthen the grid cloth docking.
 
17, the resettlement of strengthened layer construction method is the same as the standard of screen.
 
18, metope stickup grid cloth should be covered in the package grid cloth.
 
19 from top to bottom, mesh cloth wipe, synchronous construction first wipe reinforced net cloth, do standard mesh cloth
 
After 20, mesh cloth glued should prevent the rains washed out or impact, easy to collision, the Angle of the doors and Windows protection measures should be taken, feeding mouth parts take pollution prevention measures, surface damage or contamination should be dealt with immediately.
 
Layer 4 hours after 21, construction can't be the rain.
 
22, water protection layer after the final set timely maintenance, day and night when the average temperature is higher than 15 ℃ shall not be less than 48 hours, below 15 ℃ shall not be less than 72 hours.

General specification:
Low mesh area: 5 mm x 5 mm to 4 mm * 4 mm 3 mm * 3 mm,2.8mm*2.8mm
 
Low per square weight: 60 grams - 160 grams
 
Low volume per length: 50 m, 100 m or 200 m
 
Low per roll width: 1 m, 2 m
 
* color: white (standard) blue green or other colors
 
Low packaging: each roll of blister packaging, four or six roll a carton, a 40 foot container can hold 80000-150000 square meters
 
Low special specifications and special packaging can be made according to customer's booking